品牌 | 吉力士 |
货号 | 37 |
用途 | 玩具 消费品应用领域 |
牌号 | G7920-9001-00 |
型号 | G7920-9001-00 |
品名 | TPE |
外形尺寸 | 25/kg |
生产企业 | Avient Corporation |
是否进口 | 是 |
总览 | ||||
材料状态
|
|
|||
资料 1
|
|
|||
搜索 UL 黄卡
|
|
|||
供货地区
|
|
|||
特性
|
|
|||
用途
|
|
|||
机构评级
|
|
|||
RoHS 合规性
|
|
|||
外观
|
|
|||
形式
|
|
|||
加工方法
|
|
物理性能 |
额定值
|
单位制
|
测试方法
|
密度 / 比重
|
1.01
|
g/cm3
|
ASTM D792 |
硬度 |
额定值
|
单位制
|
测试方法
|
肖氏硬度 (邵氏 A, 10 秒)
|
21
|
|
ASTM D2240 |
弹性体 |
额定值
|
单位制
|
测试方法
|
抗张强度 3, 4 (断裂, 23°C)
|
3.21
|
MPa
|
ASTM D412 |
伸长率 3, 4 (断裂, 23°C)
|
790
|
%
|
ASTM D412 |
充模分析 |
额定值
|
单位制
|
测试方法
|
表观粘度 (200°C, 11200 sec^-1)
|
6.90
|
Pa·s
|
ASTM D3835 |
补充信息 | |||
Dynaflex™ G7920-9001-00 can be recycled as a filler or impact modifier for polyolefins, or can be recycled by grinding and reintroduction to the molding process. Similar to PP or PE recycling process, if separated appropriately, it can be recycled many times.
Municipality waste stream recycle code is "7" which is designated for "Other". Please contact GLS Thermoplastic Elastomers for a copy of our Recyclability Compliance letter. |
注射 |
额定值
|
单位制
|
|
建议的*回制料比例
|
20
|
%
|
|
料筒后部温度
|
160 到 188
|
°C
|
|
料筒中部温度
|
177 到 193
|
°C
|
|
料筒前部温度
|
188 到 210
|
°C
|
|
射嘴温度
|
188 到 216
|
°C
|
|
模具温度
|
16 到 38
|
°C
|
|
背压
|
0.172 到 0.827
|
MPa
|
|
螺杆转速
|
40 到 100
|
rpm
|
|
注射说明 | |||
Color concentrates with polypropylene (PP), ethylene vinyl acetate (EVA), or low density polyethylene (PE) carriers are most suitable for coloring Dynaflex™ G7920-9001-00. Improved color dispersion can be achieved by using higher melt flow concentrates (with a melt flow from 25 - 40 g/10 min). Typical loadings for color concentrates are 1% to 5% by weight. Liquid color can be used, but mineral oil based carriers may have a significant effect on the final hardness value. Concentrates based on PVC should not be used. A high color match consistency can be obtained by using precolored compounds available from GLS. The final determination of color concentrate suitability should be determined by customer trials.
Purge thoroughly before and after use of this product with a low flow (0.5 - 2.5 MFR) polyethylene (PE) or polypopylene (PP). Regrind levels up to 20% can be used with Dynaflex™ G7920-9001-00 with minimal property loss, provided that the regrind is free of contamination. To minimize losses during molding, the melt temperature should remain as low as possible. The final determination of regrind effectiveness should be determined by the customer. Dynaflex™ G7920-9001-00 has excellent melt stability. Maximum residence times may vary, depending on the size of the barrel. Generally, the barrel should be emptied if it is idle for periods of 8 - 10 minutes or longer. Drying is not Required Injection Speed: 1 to 3 in/sec 1st Stage - Boost Pressure: 200 to 900 psi 2nd Stage - Hold Pressure: 50% of Boost Hold Time (Thick Part): 3 to 10 sec Hold Time (Thin Part): 1 to 3 sec |